Highly sensitive giant magnetoimpedance in a solenoid containing FeCo-based ribbon

Fang Yun-Zhang(方允樟)a)b)†, Xu Qi-Ming(许启明)a)‡, Zheng Jin-Ju(郑金菊)b), Wu Feng-Min(吴锋民)b), Ye Hui-Qun(叶慧群)b), Si Jian-Xiao(斯剑霄)b), Zheng Jian-Long(郑建龙)b), Fan Xiao-Zhen(范晓珍)b), and Yang Xiao-Hong(杨晓红)c)   

  1. a. School of Material Science and Engineering, Xi醤 University of Architecture and Technology, Xi醤 710055, China;
    b. Research Center for Light Emitting Diodes, Zhejiang Normal University, Jinhua 321004, China;
    c. Jinhua Polytechnic, Jinhua 321007, China
  • Received:2011-05-29 Revised:2011-08-20 Online:2012-02-15 Published:2012-02-15
  • Contact: Xu Qi-Ming,xuqiming723@163.com; Fang Yun-Zhang,fyz@zjnu.cn E-mail:xuqiming723@163.com; fyz@zjnu.cn
  • Supported by:
    Project supported by the National Natural Science Foundation of China (Grant Nos. 50871104 and 11079029), the Natural Science Foundation of Zhejiang Province, China (Grant Nos. Y4080324 and Y6110246), and the Natural Science Foundation of Shanxi Province, China (Grant No. Sj08e101).

Abstract: The highly sensitive giant magneto-impedance effect in a solenoid containing a magnetic core of Fe36Co36Nb4Si4.8B19.2 (FeCo-based) ribbon under a weak magnetic field (WMF) is presented in this paper. The FeCo-based amorphous ribbon is prepared by single roller quenching and annealed with Joule heat in a flowing nitrogen atmosphere. The giant magnetoimpedance effect in solenoid (GMIES) profiles are measured with an HP4294A impedance analyzer. The result shows that the GMIES responds to the WMF sensitively (as high as 1580 %/A$\cdot$m-1). The high sensitivity can be obtained in a moderate narrow range of annealing current density (30-34 A/mm2) and closely depends on the driven current frequency. The highest sensitivity (1580 %/A$\cdot$m-1) is obtained when the FeCo-based amorphous ribbon is annealed at 32 A/mm2 for 10 min and then driven with an alterning current (AC) at the frequency of 350 kHz. The highly sensitive GMIES under the WMF may result from the multiple magnetic-anisotropic structure, which is induced by the temperature gradient produced during Joule-heating the ribbon.

Key words: giant magneto-impedance, FeCo-based ribbon, Joule heat, weak magnetic field

中图分类号:  (Metals and alloys)

  • 75.20.En
75.47.Np (Metals and alloys) 75.50.Bb (Fe and its alloys) 75.50.Gg (Ferrimagnetics)