中国物理B ›› 2018, Vol. 27 ›› Issue (9): 96501-096501.doi: 10.1088/1674-1056/27/9/096501
• CONDENSED MATTER: STRUCTURAL, MECHANICAL, AND THERMAL PROPERTIES • 上一篇 下一篇
Li-Min Zhao(赵利敏), Yong-Guang Cheng(程永光), Hao-Shan Hao(郝好山), Jiao Wang(王娇), Shao-Hui Liu(刘少辉), Bao-Sen Zhang(张宝森)
Li-Min Zhao(赵利敏), Yong-Guang Cheng(程永光), Hao-Shan Hao(郝好山), Jiao Wang(王娇), Shao-Hui Liu(刘少辉), Bao-Sen Zhang(张宝森)
摘要:
β-eucryptite powders are prepared by the sol-gel method through using tetraethoxysilane lithium nitrate and aluminum isopropoxide as starting materials. β-eucryptite ceramics are prepared by spark plasma sintering. The effects of sintering temperature on the negative thermal expansion properties of the β-eucryptite are investigated by x-ray diffraction (XRD), scanning electron microscopy, and thermal expansion test. The XRD results exhibit no change in the crystal structure of the sample prepared by different sintering processes. The negative thermal expansion properties increase with the increase of the sintering temperature. The coefficient of thermal expansion of β-eucryptite ceramics sintered at 1100 ℃ is calculated to be -4.93×10-6 ℃-1. Crystallization behaviors of the ceramics may play an important role in the increase of negative thermal expansion of β-eucryptite. High sintering temperature could improve the crystallization behaviors of the ceramics and reduce the residue glass phase, which can improve the negative thermal expansion properties of β-eucryptite ceramics.
中图分类号: (Thermal expansion; thermomechanical effects)