摘要: With annealing temperature kept at 1573 K, the effects of annealing time on stability of the intrinsic defects in epitaxial unintentionally doped 4H-SiC prepared by low pressure chemical vapour deposition have been studied by electron spin resonance (ESR) and low temperature photoluminescence. This paper reports the results shown that annealing time has an important effect on the intrinsic defects in unintentionally doped 4H-SiC when annealing temperature kept at 1573 K. When the annealing time is less than 30 min, the intensity of ESR and photoluminescence is increasing with annealing time prolonged, and reaches the maximum when annealing time is 30 min. Then the intensity of ESR and photoluminescence is rapidly decreased with the longer annealing time, and much less than that of as-grown 4H-SiC when annealing time is 60 min, which should be related with the interaction among the intrinsic defects during the annealing process.
中图分类号: