Congruent melting of tungsten phosphide at 5 GPa and 3200 °C for growing its large single crystals
Xiang Xiao-Jun1, 2, Song Guo-Zhu3, Zhou Xue-Feng3, Liang Hao1, Xu Yue5, Qin Shi-Jun2, 4, Wang Jun-Pu1, Hong Fang2, Dai Jian-Hong3, Zhou Bo-Wen2, 4, Liang Wen-Jia1, Yin Yun-Yu2, Zhao Yu-Sheng3, Peng Fang1, †, Yu Xiao-Hui2, ‡, Wang Shan-Min3, §
       

(a) Determined TG-DTA data for polycrystalline WP. (b) XRD patterns of the sample treated at 1400 °C to look into decomposition process of panel (a).