Regulation mechanism of catalyst structure on diamond crystal morphology under HPHT process
Li Ya-Dong1, Cheng Yong-Shan1, Su Meng-Jie1, Ran Qi-Fu1, Wang Chun-Xiao2, Ma Hong-An2, Fang Chao3, Chen Liang-Chao3, †
       

Diamonds synthesized on CHPA with Fe–Ni catalyst under 5.7 GPa and 1310 °C for (a) mode A, (b) mode B, and (c) mode C.