Xu Qing-Jun1, 2, Zhang Shi-Ying1, 2, Liu Bin1, ‡, Li Zhen-Hua1, 2, Tao Tao1, Xie Zi-Li1, §, Xiu Xiang-Qian1, Chen Dun-Jun1, Chen Peng1, Han Ping1, Wang Ke1, Zhang Rong1, Zheng You-Liao1
       

(a) CL peak position (Eemi) of present impurity transition (solid stars) observed from Fig. 1 and those of (VIII complex)1− related transitions (solid squars) obtained from undoped AlxGa1 − xN alloys as a function of AlN mole fraction x in Ref. [16]; (b) EA versus AlN mole fraction for (VIII-complex)1−, Ev, Ec, and ED.