In situ
luminescence measurement of 6H-SiC at low temperature
Qiu Meng-Lin
1
, Yin Peng
1
, Wang Guang-Fu
1, 2, †
, Song Ji-Gao
1
, Luo Chang-Wei
1
, Wang Ting-Shun
1
, Zhao Guo-Qiang
1
, Lv Sha-Sha
1
, Zhang Feng-Shou
1, 2
, Liao Bin
1
The FWHM evolution of the fitted peaks at 1.79 eV and 2.14 eV with fluence at 150 K.