(a)–(h) SEM images of Y2−x(LiZn)xMo3O12 with x = 0, 0.3, 0.7, 1.0, 1.2, 1.4, 1.6, 1.8, and 2.0. The grain shapes change remarkably with increasing the content of (LiZn)3+.