Shen Xiong1, Feng Guo-Ying1, Jing Sheng2, Han Jing-Hua1, †, Li Ya-Guo3, Liu Kai1
       

Damage morphologies of 1-mm-thick fused silica surface under different numbers of pulses: (a) 1 pulse; (b) 3 pulses; (c) 5 pulse; (d) 10 pulses; (e) 15 pulses; (f) 20 pulses.