Effects of CeO2 and nano-ZrO2 agents on the crystallization behavior and mechanism of CaO–Al2O3–MgO–SiO2-based glass ceramics
Zhang Yan1, 2, Shi Yu3, Zhang Xuefeng3, Hu Fengxia1, 2, Sun Jirong1, 2, Zhao Tongyun1, 2, Shen Baogen1, 2, †
       

Scanning thermal analysis (DSC) curves of samples (a) A, (b) B, and (c) C in different heating rates. The inset of panel (c) is an enlarged view of the DSC curve at the heating rate of 10 °C/min between 600 °C and 800 °C. (d) ln(Tp2/ξ) vs. 1/Tp and the corresponding linear fittings (straight lines) of the three samples.