Influence of annealing treatment on the luminescent properties of Ta:β-Ga2O3 single crystal
Yu Xiaowei1, Cui Huiayuan2, Zhu Maodong2, Xia Zhilin1, †, Sai Qinglin2, ‡
       

PL decay profiles of 0.01 mol% Ta:β-Ga2O3 before and after annealing measured under excitation of 256 nm. The monitoring wavelengths are (a) 370 nm and (b) 420 nm. The lines indicate the fitting curves.