Regulating element distribution to improve magnetic properties of sintered Nd–Fe–B/Tb–Fe–B composite magnets
Li Zhu-Bai1, 2, †, Zuo Jing-Yan1, Wang Dong-Shan2, Liu Fei1, 2, Zhang Xue-Feng1, 2
       

The surface micromorphology of the sintered magnets of (a) Nd13.2Fe80.8B6/Tb17Fe75B8, (b) Nd12.7Fe81.3B6/Tb17Fe75B8, (c) Nd12.2Fe81.8B6/Tb17Fe75B8, and (d) Nd11.7Fe82.3B6/Tb17Fe75B8.