Improved electrochemical performance of Li(Ni0.6Co0.2Mn0.2)O2 at high charging cut-off voltage with Li1.4Al0.4Ti1.6(PO4)3 surface coating
Wang Yi1, 2, Liu Bo-Nan3, Zhou Ge1, 2, Nie Kai-Hui1, 2, Zhang Jie-Nan1, ‡, Yu Xi-Qian1, 2, †, Li Hong1, 2, 3
       

(a) The DSC and (b) TG curves for bare NCM622 and LATP-NCM-600 electrodes after the first charge to 4.5 V.