Low temperature Pmmm and C2/m phases in Sr2CuO3+δ high temperature superconductor
Wang Hai-Bo1, Luo Zhen-Lin2, ‡, Yang Yuan-Jun2, Liu Qing-Qing3, Hu Si-Xia2, Yang Meng-Meng2, Jin Chang-Qing3, Gao Chen2, 4, †
       

X-ray diffraction result of Sr2CuO3+δ as function of temperature and incident x-ray energy. (a) and (b) The x-ray diffraction patterns obtained at varied temperatures with x-ray energy of (a) 8.500 keV and (b) 8.990 keV. Some modulated structures emerge in the low temperature region.