Structural evolution in deformation-induced rejuvenation in metallic glasses: A cavity perspective
Jiang Shaoqin, Huang Yong, Li Maozhi
       

The evolution of (a) total volume and (b) total number of cavities of four different specimens as a function of temperature from 2000 K to 300 K.