Review of photoresponsive properties at SrTiO3-based heterointerfaces
Yan Hong, Zhang Zhaoting, Wang Shuanhu, Jin Kexin †
(color online) Variation of the relative change in the resistance () with the time for 8 nm thick LaTiO3 (LTO) (open symbols) and LAO (filled symbols) deposited at different temperatures on (100) STO substrates. These measurements were done at room temperature.[38]