Rare earth permanent magnets prepared by hot deformation process |
TEM images and electron diffraction SAED patterns of amorphous Nd9Fe85B6 alloy (a) subjected to HPTD and subsequently annealed at 600 °C for 10 min and (b) directly annealed at 725 °C for 10 min.[ |