Mn-based permanent magnets
Yang Jinbo1, 2, 3, †, Yang Wenyun1, 2, 3, Shao Zhuyin1, 2, 3, Liang Dong1, 2, 3, Zhao Hui1, 2, 3, Xia Yuanhua4, Yang Yunbo1
       

XRD patterns of the Mn54Al46 alloys prepared with method (ii) (melt spinning speed is 30 m/s) at different steps (a)–(c).