Mn-based permanent magnets
Yang Jinbo1, 2, 3, †, Yang Wenyun1, 2, 3, Shao Zhuyin1, 2, 3, Liang Dong1, 2, 3, Zhao Hui1, 2, 3, Xia Yuanhua4, Yang Yunbo1
       

(color online) XRD patterns of Mn54−xAl46Cx (x = 0, 1, 2, 3) ingots annealed at 1050 °C for two days and then cooled to room temperature.