Mn-based permanent magnets
Yang Jinbo1, 2, 3, †, Yang Wenyun1, 2, 3, Shao Zhuyin1, 2, 3, Liang Dong1, 2, 3, Zhao Hui1, 2, 3, Xia Yuanhua4, Yang Yunbo1
       

XRD patterns of the MnBi after melt spinning at a speed of 65 m/s (a) and subsequently annealing at 573 K for 3 h (b).[38]