Mn-based permanent magnets
Yang Jinbo1, 2, 3, †, Yang Wenyun1, 2, 3, Shao Zhuyin1, 2, 3, Liang Dong1, 2, 3, Zhao Hui1, 2, 3, Xia Yuanhua4, Yang Yunbo1
       

(color online) Room temperature M(H) hysteresis loops of Mn54.5Al45.5−xGax (x = 0.0, 15.0, 25.0, 35.0, 45.5) samples. The inset shows the coercivity as a function of Ga content with milling time of 0 and 30 min.[18]