Nanocrystalline and nanocomposite permanent magnets by melt spinning technique
Rong Chuanbing1, †, Shen Baogen2
       

(color online) The 2D and 3D FORC diagrams of the samples (a) without milling, and milled for (b) 30, (c) 60, and (d) 240 minutes after annealing at 525 °C for 30 minutes. Left column is the colored FORC curves with the FORC distribution plotted inside the hysteresis loop. The middle column is the 2D FORC diagrams and right column is 3D FORC diagrams.[272]