Fabrication of Tl2Ba2CaCu2O8 superconducting films without thallium pellets |
(color online) SEM micrographs of Tl-2212 films annealed under different conditions: (a) at 750 °C for 120 min, (b) at 760 °C for 120 min, (c) at 760 °C for 180 min, (d) at 810 °C for 120 min. |