Fabrication of Tl2Ba2CaCu2O8 superconducting films without thallium pellets
Xu Teng-Da1, Xing Jian1, Wang Li-Tian1, Zhang Jin-Li1, Zhao Sheng-Hui1, Xiong Yang1, Zhao Xin-Jie1, 2, Ji Lu1, 2, †, Zhang Xu1, He Ming1
       

(color online) XRD patterns of Tl-2212 films prepared with different annealing conditions: (a) at 750 °C for 120 min, (b) at 770 °C for 120 min, (c) at 790 °C for 120 min, (d) at 770 °C for 240 min.