Polycrystalline cubic boron nitride prepared with cubic-hexagonal boron nitride under high pressure and high temperature
Yang Ming1, Kou Zi-Li1, †, Liu Teng1, Lu Jing-Rui1, Liu Fang-Ming2, Liu Yin-Juan1, Qi Lei1, Ding Wei1, Gong Hong-Xia1, Ni Xiao-Lin1, He Duan-Wei1
       

(color online) (a) Vickers hardness of samples sintered at 6.5–10.0 GPa/1750 °C with an applied load of 29.4 N. Inset: micrograph of Vickers hardness indentation. (b) Applied load dependence of Vickers hardness of the sample sintered at 7.7 GPa/1750 °C.