Polycrystalline cubic boron nitride prepared with cubic-hexagonal boron nitride under high pressure and high temperature
Yang Ming1, Kou Zi-Li1, †, Liu Teng1, Lu Jing-Rui1, Liu Fang-Ming2, Liu Yin-Juan1, Qi Lei1, Ding Wei1, Gong Hong-Xia1, Ni Xiao-Lin1, He Duan-Wei1
       

(color online) (a) XRD patterns of starting material and samples hBN content of the starting materials (range from 16 vol.% to 28 vol.%) sintered at 7.5 GPa/1750 °C. (b) XRD patterns of starting material and samples (20 vol.%-hBN) sintered at 6.5–10.0 GPa/1750 °C.