Low-temperature synthesis of apatite-type La9.33Ge6O26 as electrolytes with high conductivity
Yin Guang-Chao1, Zhao Guo-Dong1, Yin Hong2, Jia Fu-Chao1, Jing Qiang1, Fu Sheng-Gui1, Sun Mei-Ling1, †, Gao Wei2, ‡
       

(color online) Arrhenius plots for the conductivity of La9.33Ge6O26 pellets sintered by MSSM at 1100 °C and the compared pellets sintered by SSRM at 1300 °C.