Wang Hao1, 2, Chen Jin1, 2, Lu Tianqi2, Zhu Kunjie1, Li Shan2, Liu Jun1, †, Zhao Huaizhou2, ‡
|
(color online) (a) Room-temperature Hall carrier concentration and Hall mobility of Mg3−xLixSb2 (x = 0, 0.005, 0.01, 0.02), (b) the Seebeck coefficient versus carrier concentration at room temperature. The black solid curve is the calculated relation between Seebeck coefficient and carrier concentration using an SPB model with
m*=0.76me
, while the scatters represent the experimental data of Mg3−xLixSb2 (x = 0, 0.005, 0.01, 0.02) compounds.
|