Thermomechanical response of aluminum alloys under the combined action of tensile loading and laser irradiations |
(color online) Failure behavior of the Al-7075 specimens as a function of pre-loaded values under fixed laser power densities: (a) 1.5 kW/cm2, (b) 1.9 kW/cm2, (c) 2.3 kW/cm2, and (d) 2.7 kW/cm2. |