ul Hassan Najam1, Ahmad Shah Ishfaq1, Khan Tahira2, Liu Jun1, Gong Yuanyuan1, Miao Xuefei1, Xu Feng1, †
|
(color online) M–B curves at various temperatures around the martensitic transformation for the Mn48−xVxNi42Sn10: (a) x = 0, (b) x = 1, and (c) x = 2. (d) High field M–T curves for Mn48−xVxNi42Sn10 (x = 0, 1, and 2) alloys with a magnetic field of 3 T (open symbols) and 5 T (solid symbols) in the heating process.
|