Influences of substrate temperature on microstructure and corrosion behavior of APS Ni50Ti25Al25 inter-metallic coating
Khandanjou Sh1, Ghoranneviss M1, Saviz Sh1, †, Afshar M Reza2
       

Vickers test traces in the coating-substrate interface at substrate temperatures of (a) room temperature, (b) 200 °C, and (c) 400 °C.