Gas treatment protection of metallic lithium anode
Li Wen-jun1, 2, Li Quan1, 2, Huang Jie1, 2, Peng Jia-yue1, 2, Chu Geng1, 2, Lu Ya-xiang1, Zheng Jie-yun1, Li Hong1, †
       

(color online) Current distribution (obtained by SPM) of lithium tablets treated by argon (a), CO2–O2 (2:1) (b), N2 (c), and CO2–O2–N2 (2:1:3) (d) gases respectively.