Molecular dynamics simulations of cascade damage near the Y2Ti2O7 nanocluster/ferrite interface in nanostructured ferritic alloys
Sun Yi-Qiang, Lai Wen-Sheng
       

(color online) Variations of the number of surviving defects in the matrix of the NFA with Ep for the different PKA positions at (a) d = 10Å, (b) 20 Å, and (c) 30 Å after 20 ps. The black line obtained in pure Fe is also shown for comparison.