A low cost composite quasi-solid electrolyte of LATP, TEGDME, and LiTFSI for rechargeable lithium batteries
Huang Jie1, 2, Peng Jia-Yue1, 2, Ling Shi-Gang1, 2, Yang Qi1, 2, Qiu Ji-Liang1, 2, Lu Jia-Ze1, 2, Zheng Jie-Yun1, 2, Li Hong1, 2, †, Chen Li-Quan1, 2
       

(color online) The variations of the ionic conductivities for CQSE and QSE membranes with 70, 60, 50 vol% of [LiG4][TFSI] in the temperature range of 10 °C∼50 °C.