Serrated magnetic properties in metallic glass by thermal cycle
Ri Myong-Chol1, 3, Sohrabi Sajad1, 3, Ding Da-Wei1, †, Dong Bang-Shao2, Zhou Shao-Xiong2, Wang Wei-Hua1, ‡
       

(color online) Cryogenic thermal cycling procedure of metallic glass. Samples are cycled from near room temperature (300 K) to liquid nitrogen temperature (77 K). At each end the holding time is 1 min, so one cycle time is 2 min. Due to inertia of thermal energy the edge is not sharp. The degree of dullness and stabilization are different due to the sizes of samples