CuO added Pb0.92Sr0.06Ba0.02(Mg1/3Nb2/3)0.25(Ti0.53Zr0.47)0.75O3 ceramics sintered with Ag electrodes at 900 °C for multilayer piezoelectric actuator*

Project supported by the National Natural Science Foundation of China (Grant Nos. 51472118, 51602156, 52177072, and 11274174) and the Fundamental Research Funds for the Central Universities, China (Grant Nos. 30916011104 and 30916011208).

Qaiser Muhammad Adnan1, Hussain Ahmad1, Xu Yuqing1, Wang Yaojin1, Wang Yiping2, Yang Ying2, Yuan Guoliang1, †
       

(color online) PE loops of x CuO added ceramics with x = 03 wt.% (a), 0.5 wt.% (b), 0.7 wt.% (c), 0.9 wt.% (d) sintered at 850 °C, 900 °C, 950 °C, 1000 °C, and 1050 °C.