Room temperature NO2-sensing properties of hexagonal tungsten oxide nanorods
Wu Yaqiao1, 2, Hu Ming1, †, Tian Yuming2
       

(color online) Dynamic responses of the gas sensors based on the WO3 nanorods annealed at (a) 300 °C, (b) 400 °C, and (c) 500 °C to varying NO2 concentration at room temperature. (d) Relationship between the responses and NO2 concentration for the sensors based on annealed tungsten WO3 nanorods at room temperature.