Hot corrosion behavior of the spray-formed nickel-based superalloy |
Microstructures and EDS analyses of the surface corrosion products of spray-formed FGH100 tested for 100 h: ((a), (c), and (e)) the surface appearance of corroded samples; ((b), (d), and (f)) EDS result of the corrosion products in panels (a), (c), and (e) respectively. |