Hot corrosion behavior of the spray-formed nickel-based superalloy
Xia Min1, †, , Gu Tian-Fu1, Jia Chong-Lin1, 2, Ge Chang-Chun1, ‡,
       

XRD patterns of the surface corrosion products of spray-formed FGH100, tested at 700 °C for 1 h and 10 h, 100 h.