Effects of thickness and annealing condition on magnetic properties and thermal stabilities of Ta/Nd/NdFeB/Nd/Ta sandwiched films
Liu Wen-Feng
1
, Zhang Min-Gang
1, †,
, Zhang Ke-Wei
1
, Zhang Hai-Jie
1
, Xu Xiao-Hong
2
, Chai Yue-Sheng
1
Hysteresis loops of Ta/Nd(250 nm)/NdFeB (600 nm)/Nd(250 nm)/Ta films annealed at 1023 K.