Effects of thickness and annealing condition on magnetic properties and thermal stabilities of Ta/Nd/NdFeB/Nd/Ta sandwiched films |
Dependences of the (a) in-plane and (b) out-of-plane coercivities on Nd layer thickness in Ta/Nd/NdFeB(600 nm)/Nd/Ta films annealed for 30 min at different temperatures. |