Magnetoresistance and exchange bias in high Mn content melt-spun Mn46Ni42Sn11Sb1 alloy ribbon
Huang Qingxue1, †, , Chen Fenghua1, ‡, , Zhang Mingang1, Xu Xiaohong2
       

The Mn46Ni42Sn11Sb1 alloy ribbons annealed at 1073 K for 1 h. (a) SEM micrograph of ribbon fractured cross section, and (b) the room-temperature XRD pattern.