Preparation and room temperature NO2-sensing performances of porous silicon/V2O5 nanorods |
(a) NO2 concentration-dependent response values of PS/V2O5 nanorods at 25 °C. (b) Dynamic response curve of PS/V2O5 nanorods annealed at 600 °C for 30 min to various concentrations of NO2 at 25 °C. |