Influences of spark plasma sintering temperature on the microstructures and thermoelectric properties of (Sr |
XRD patterns of SGTO powders annealed at 1473 K (before SPS) and SGTO ceramics SPSed at 1548 K (S1548), 1648 K (S1648), and 1748 K (S1748) respectively. |