Effects of oxidation of DyH3 in Nd–Fe–B sintered magnets
Yan Gao-Lin†, Fang Zhi-Hao
       
The macroscopic corrosion status and microstructures of magnets of samples I, II, and III after corrosion at 85 °C, RH: 80% in the environmental chamber for 18 days.