Pressure effect on magnetic phase transition and spin-glass-like behavior of GdCo2B2
Hu Guang-Hui1, †, , Li Ling-Wei2, Izuru Umehara1
       

Temperature dependence of ZFC magnetization with intermittent stops at 2, 3, and 4 K for 1800 s (empty symbols) and that of a normal ZFC process (solid symbols).